Mechanical
- Tensile strength
- 38 MPa
- Elongation at break
- 6 %
- Flexural strength
- 58 MPa
- Flexural modulus
- 1600 MPa
- Izod impact (notched)
- 18 J/m
- Shore hardness
- 79D
- Compressive strength
- 54 MPa
Thermal
- HDT @ 0.45 MPa
- 56 °C
- HDT @ 1.82 MPa
- 46 °C
- Glass transition
- 60 °C
- Max service temp
- 48 °C
Curing & print
- Viscosity @ 25°C
- 320 cP
- Cure wavelength
- 385-405nm nm
- Post-cure
- 15 min UV post-cure
- Shrinkage / accuracy
- 0.80%
- Water-washable
- No
Physical
- Density
- 1.11 g/cm³
- Available colors
- Red
- Biocompatibility
- Ash-free investment casting formulation