HARZ Labs
Dental Cast
Castable
Direct investment casting of crowns, copings, dental frameworks; LCD/DLP
Full specifications
Mechanical
- Tensile strength
- 48 MPa
- Elongation at break
- 5 %
- Flexural strength
- 70 MPa
- Flexural modulus
- 1700 MPa
- Izod impact (notched)
- 15 J/m
- Shore hardness
- 76D
- Compressive strength
- 56 MPa
Thermal
- HDT @ 0.45 MPa
- 58 °C
- HDT @ 1.82 MPa
- 46 °C
- Glass transition
- 62 °C
- Max service temp
- 48 °C
Curing & print
- Viscosity @ 25°C
- 420 cP
- Cure wavelength
- 385nm / 405nm nm
- Post-cure
- Minimal post-cure before investment
- Shrinkage / accuracy
- 0.90%
- Water-washable
- No
Physical
- Density
- 1.1 g/cm³
- Available colors
- Red Translucent
- Biocompatibility
- Zero ash residue burnout (<0.1%)