Ameralabs
TGM-7 Flexible
Flexible/Elastomeric
Mixing resin to eliminate brittleness, impact dampeners; Open 385-405nm LCD/DLP
Full specifications
Mechanical
- Tensile strength
- 20 MPa
- Elongation at break
- 110 %
- Shore hardness
- 75A
Thermal
- Glass transition
- -12 °C
- Max service temp
- 46 °C
Curing & print
- Viscosity @ 25°C
- 880 cP
- Cure wavelength
- 385-405nm nm
- Post-cure
- 20 min UV in water
- Shrinkage / accuracy
- 2.00%
- Water-washable
- No
Physical
- Density
- 1.1 g/cm³
- Available colors
- Clear
- Biocompatibility
- Non-brittle flexible resin additive